Surface chemical and color characterization of juvenile tectona grandis wood subjected to steam-drying treatments

2016

Berrocal, A., Moya, R., Rodriguez-Solís, M., Starbird, R., & Muñoz, F. (2016). Surface chemical and color characterization of juvenile tectona grandis wood subjected to steam-drying treatments. Surface Review and Letters, 23(1).

Artículo

The color of Tectona grandis wood is an attribute that favors its commercialization, however, wood color from fast-growth plantation trees is clear and lacks uniformity. The aim of this work is to characterize steamed teak wood by means of the Fourier transform infrared spectroscopy (FTIR) and L a b color systems. Two moisture conditions (green and 50%) and two grain patterns (°at and quarter) of boards were analyzed through the application of di®erent steaming times (0, 3, 6, 9, 12, 15 and 18 h). The FTIR results showed that the bands at 1158, 1231, 1373 and 1419 cm 1 did not show any change with steaming, whereas the bands at 1053, 1108, 1453, 1506, 1536, 1558, 1595, 1652, 1683, 1700 and 1733 cm 1 presented a decrease in the intensity with the steaming time. The band at 1318 cm 1 was the only one that increased. Lightness (L ) was the most a®ected parameter, followed by yellowness (b ), while redness (a ) showed the smallest change. Surface color change ( E ) presented the lowest value between 3 h and 6 h of steam-drying in the boards with °at grain, whereas for boards with quarter grain, the smallest E value was obtained after 18 h of steaming.

Instituto Tecnológico de Costa Rica

Lidia Gómez

Cartago - 300m Este del Estadio Fello Meza. Apartado 159-7050.

2550-2263, 2550-2365


Dirección: Av. Mariscal Antonio José de Sucre N58-63 y Fernández Salvador Edif. Olade - San Carlos, Quito - Ecuador.

Web: www.olade.org

Teléfonos: (593 2) 259 8122 / 2598 280

Correo: realc@olade.org

ADMIN
Desarrollado por: Aikyu-Systems